#翡翠项链#翡翠吊坠#上海翡翠品牌#北京翡翠店#上海哪里买翡翠#北京哪里买翡翠#高端翡翠首饰#高档翡翠#天然翡翠#怎样鉴别好翡翠#翡翠手镯#翡翠珠宝#阳绿翡翠#翡翠8个等级#翡翠A货价格多少#翡翠最好的6种颜色#翡翠的种水有什么特点#翡翠的价值和意义#玉石翡翠#翡翠的价格和图片#翡翠的保养方法#玉石珠宝#用手机灯光鉴别翡翠#什么翡翠档次最高#翡翠的功效与作用#在哪买翡翠#哪里卖的翡翠最靠谱#适合送礼物的翡翠是哪些#青岛翡翠手镯店#大连翡翠首饰商家#苏州翡翠手镯店#重庆哪里买翡翠#武汉翡翠商家#翡翠价格#翡翠会越戴越透亮吗#翡翠真假如何区分#翡翠有裂纹能买吗#翡翠手镯怎么选圈口#翡翠手镯哪个好#5000元左右的翡翠手镯#挑选翡翠的四个口诀#翡翠最值钱的颜色#翡翠手镯在哪里买到真的#翡翠什么颜色最贵#翡翠鉴定#翡翠戴久了前后变化#真假飘花翡翠#有证书的翡翠怎么查价格#翡翠一般卖多少钱#翡翠款式有哪些#翡翠手镯可以戴着洗澡吗#翡翠寓意和象征#10万元翡翠手镯推荐#鉴别翡翠真假和好坏#翡翠耳钉多少钱一对#翡翠耳环款式#50岁女人戴哪种翡翠#哪种翡翠耳钉最有气质#戴翡翠耳钉的寓意#天然A货翡翠耳钉价格#翡翠正品#翡翠手镯正品
伴随着销售市场的发展趋势,翡翠在销售市场上愈发赚钱,翡翠的使用价值是愈来愈高,可是一样的翡翠中这些好翡翠确是越来越低,很多人为了更好地挣钱而刚开始动一些歪脑筋,因此人力翡翠就问世了,那麼假翡翠是怎样制成的呢?
假翡翠实际上也是翡翠,仅仅翡翠的品相不太好,做不了好物品儿,品相不太好的翡翠原石价格是很便宜的。因此 黑商们便会把她们全部的总是集中化起來放进这上边来,就是把垃圾池里拾来的物品让你制成a货翡翠。都说玉会以养,那这种历经各种各样生产加工的翡翠,看上去是漂亮了,但是他们能以养么?
B货翡翠的解决方式
翡翠历经补胶解决后再开展打磨抛光等事后解决,使表层光滑,光泽度提升,网状结构龟裂痕不容易出現,绚丽多彩。B货的伤害就别说了!B货翡翠会用强碱浸蚀掉翡翠表层的一些缺陷,留存下来的一些浸蚀裂缝就根据添充的方式来填补,用强碱解决过得翡翠其表层多多少少的会出现一些遗留下化学物质,这种化学物质会对身体导致多多少少的损害,所以说在挑选层面不是强烈推荐的。
翡翠B货的解决也不是随意就可以解决的,针对强酸强碱的浓度值,拆换频次这些全是拥有 一定的规定,一般来说要依据翡翠的本身使用价值及其解决后的使用价值来挑选浓度值,拆换频次这些,强酸强碱浓度值越高,生产加工的花费就越大,成本费越高当然权益就越低。
强酸强碱解决以后便是要添充了,强酸强碱解决翡翠的全过程呈顺着顆粒空隙开展的因此造成 其构造松散,填充环氧树脂不但为了更好地粉细砂已变成疏松状的构造提升 其抗压强度也为了更好地这到提升清晰度的目地。这类添充是B货翡翠处理所必然的一个方式,沒有历经添充的翡翠B货本身会出现许多 坑坑洼洼存有。会大大的危害B货翡翠的售卖。
补胶填充解决前,可依据顾客必须开展上色解决,在原材料表层点染色浆。色浆分成油溶和水溶性二种,各自称之为油溶性染剂和水溶性染剂;可点染也可沾染;可染相同色调,还可以另外染多种多样色调。上色后再开展补胶填充解决,更看起来当然温和,且平稳不容易退色。
其次就是翡翠B货解决早期的原材料挑选。开展B解决的翡翠一般挑选中低端、中粗粒构造和裂缝多的翡翠。如豆种、花青、白色背景青等原材料,而纤维细砂构造和裂缝非常少的翡翠一般不做此解决。这种翡翠通常使用价值较低,能够以非常低的价钱回收较多的货,所以说在挑选层面当然也是下手这种类型的了。
With the development trend of the sales market, jade is making more and more money in the sales market. The value of jade is getting higher and higher, but among the same jade, these good jade are getting lower and lower. Many people are just starting to use some crooked ideas to make better money, so artificial jade has emerged. So, how is fake jade made?
Fake jade is actually jade, but its appearance is not very good and it cannot be made into a good item. The price of raw jade with poor appearance is very cheap. Therefore, black merchants will concentrate all their resources and put them on top of it, which is to turn the items picked up from the garbage pit into A-grade jade. It is said that jade can be nurtured. Jade that has undergone various production and processing may look beautiful, but can they be nurtured?
Solution for B-grade jade
After the jade is repaired with adhesive, it is then polished and polished to achieve a smooth surface and improved glossiness. The mesh structure and cracks are less likely to appear, making it colorful and vibrant. Let’s not talk about the harm caused by B-goods! B-grade jadeite will use strong alkali to etch away some defects on the surface of the jadeite, and the remaining etched cracks will be filled according to the filling method. After using strong alkali to solve the problem, there will be some residual chemical substances on the surface of the jadeite, which will cause more or less damage to the body. Therefore, it is not strongly recommended in the selection process.
The solution to the problem of B-grade jadeite is not something that can be solved casually. There are certain regulations regarding the concentration values of strong acids and alkalis, as well as the frequency of replacement. Generally speaking, the concentration values should be selected based on the inherent use value of jadeite and its value after being solved. The frequency of replacement should also be determined. The higher the concentration value of strong acids and alkalis, the higher the production and processing costs, and of course, the lower the equity.
After the solution of strong acid and strong alkali, it is necessary to add them. The entire process of solving jade with strong acid and strong alkali follows the particle voids, resulting in loose structure. Filling with epoxy resin is not only to improve the loose structure of fine sand, but also to enhance its compressive strength and clarity. This type of filling is an inevitable way of processing B-grade jade, and B-grade jade that has not undergone filling itself will have many potholes and bumps. It will greatly endanger the sale of B-grade jadeite.
Before filling the adhesive, coloring can be carried out according to the customer’s requirements, and coloring paste can be applied to the surface of the raw material. Color paste is divided into two types: oil soluble and water-soluble, each referred to as oil soluble dye and water-soluble dye; Can be dyed or stained; Can be dyed in the same color tone, and can also be dyed in a variety of different colors. After coloring, apply adhesive filling to solve the problem, which looks more gentle and stable, and is not easy to fade.
Secondly, the selection of raw materials for jadeite B-grade products can be addressed in the early stages. Generally, jadeite with medium to low end, medium coarse grain structure, and many cracks are selected for B solution. Raw materials such as bean seeds, flower green, white background green, etc., while jadeite with very few fiber fine sand structures and cracks is generally not treated with this solution. This type of jade usually has low value and can be recycled at a very low price, so of course, when it comes to selection, one should also focus on this type.